Al-Mg-Si-Zr-XEr合金β″相析出动力学的研究
DOI:
作者:
作者单位:

沈阳工业大学材料科学与工程学院,沈阳工业大学材料科学与工程学院,沈阳工业大学材料科学与工程学院,沈阳市装备制造工程学校

作者简介:

通讯作者:

中图分类号:

基金项目:

辽宁省第三批特聘教授支持计划


The Study on Precipitation Kinetics for β″ Phase of Al-Mg-Si-Zr-XEr Alloy
Author:
Affiliation:

School of Materials Science and Engineering,Shenyang University of Technology,School of Materials Science and Engineering,Shenyang University of Technology,School of Materials Science and Engineering,Shenyang University of Technology,Shenyang Equipment Manufacturing Engineering School

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    通过组织观察、性能检测和差热分析(DSC)试验,研究了不同Er元素含量下Al-Mg-Si-Zr-XEr合金时效硬化曲线、TEM组织、β″相的析出激活能和TTT曲线,并得到对应的β″相析出动力学方程和TTT表达式。研究结果表明:Er元素的添加促进了β″相的析出,在540 ℃固溶1 h 180 ℃时效5 h时,Al-Mg-Si-Zr-0.3Er合金中的β"相细小均匀的弥散析出;随Er元素含量增加,合金硬化速率明显加快,软化速率降低,合金β″相析出激活能降低,分别为96.3、93.6和84.9 kJ/mol;析出动力学方程分别为:YEr0.1=1-exp[-1.534×1013t1.5exp(-17382.7/T)]、YEr0.2=1-exp[-5.865×1012t1.5exp(-16895.3/T)]、YEr0.3=1-exp[-2.965× 1011t1.5exp(-15324.9/T)];TTT曲线方程分别为:TEr0.1=17382.7/[30.4 1.5lnt-lnln(1-Y)-1]、TEr0.2=16895.3/[29.4 1.5lnt-lnln(1-Y)-1]、TEr0.3=15324.9/[26.4 1.5lnt-lnln(1-Y)-1]。

    Abstract:

    By means of performance testing, microstructure and differential thermal analysis, the hardness-time curves, TEM microstructures, TTT curves and precipitate activation energy of β″ phase for Al-Mg-Si-Zr-XEr alloy were investigated, and kinetics expressions and TTT expressions of β″ phase were acquired. The results show that the addition of Er element accelerates the dispersively precipitation of the β″ phase, and the fine and uniform β″ phase of Al-Mg-Si-Zr-0.3Er alloy precipitate dispersively after the solution treatment at 540 ℃ for 1 h and aging at 180 ℃ for 5 h. As the element Er content increases, hardening rate of alloy is significantly accelerated, softening rate of alloy is decreased, precipitate activation energy of β″ phase for alloy is decreased, and the values are 96.3, 93.6 and 84.9 kJ/mol. The kinetics expressions are obtained as follows, YEr0.1=1-exp[-1.534×1013t1.5exp(-17382.7/T)], YEr0.2=1-exp[-5.865×1012t1.5exp(-16895.3/T)], YEr0.3=1-exp[-2.965×1011t1.5exp(-15324.9/ T)]. The TTT expressions are obtained as follows, TEr0.1=17382.7/[30.4 1.5lnt-lnln(1-Y)-1], TEr0.2=16895.3/[29.4 1.5lnt-lnln(1-Y)-1], TEr0.3=15324.9/[26.4 1.5lnt-lnln(1-Y)-1].

    参考文献
    相似文献
    引证文献
引用本文

赵倩,袁晓光,黄宏军,赵鹏. Al-Mg-Si-Zr-XEr合金β″相析出动力学的研究[J].稀有金属材料与工程,2016,45(11):2889~2894.[Zhao Qian, Yuan Xiaoguang, Huang Hongjun, Zhao Peng. The Study on Precipitation Kinetics for β″ Phase of Al-Mg-Si-Zr-XEr Alloy[J]. Rare Metal Materials and Engineering,2016,45(11):2889~2894.]
DOI:[doi]

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2015-12-08
  • 最后修改日期:2016-01-15
  • 录用日期:2016-02-24
  • 在线发布日期: 2016-12-08
  • 出版日期: