Effects of Nickel Content on Microstructural Evolution and γ′ Dissolution of Co-8.8Al-9.8W Base Alloys
Author:
Affiliation:

Lanzhou University of Technology,State Key Laboratory of Advanced Processing and Recycling of Non-ferrous Metals,Lanzhou University of Technology,State Key Laboratory of Advanced Processing and Recycling of Non-ferrous Metals,Lanzhou University of Technology,State Key Laboratory of Advanced Processing and Recycling of Non-ferrous Metals

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    为了研究镍含量对Co-Al-W基高温合金时效组织演变及γ′强化相溶解行为的影响,运用SEM、XRD等对时效处理后合金的γ′相微观组织形貌演变、微观组织结构、γ′相强化相转变温度和显微硬度进行了研究。结果表明,Ni含量增加,γ′相溶解温度出现不同程度的提高,γ′相的体积分数逐渐增加。但合金固相线温度和γ′相的形貌保持未发生明显变化。当Co-8.8Al-9.8W合金中镍含量达到25%(at.%)时,γ′强化相的溶解温度达到了1100℃。四种合金经900℃/50h热处理后,基体均为典型的γ/γ′两相组织。合金经900℃/100h热处理后,Ni含量增加,γ′相的体积分数均出现不同程度的降低,且γ′相发生了明显的粗化。对四种合金900 ℃, 50 h 和 100 h的显微硬度测量结果表明,当Ni含量由5%升高至15%时,其显微硬度升高;但Ni含量进一步增加,合金的显微硬度却降低。随着合金的时效处理时间由50h延长至100h,导致Co-8.8Al-9.8W基合金的显微硬度降低。

    Abstract:

    To study the effects of nickel content on microstructural evolution and γ′ dissolution of Co-Al-W base alloys, the microstructure,γ′ precipitates transformation temperatures, γ′ precipitates microstructural evolution and microhardness of Co-Al-W base alloys with aging treatment were analyzed by using scanning-electron microscope(SEM) and X-ray diffraction(XRD) etc. The results showed that with the increase of Ni,γ ′ solvus temperature increased at different degree and the volume fraction of γ′ precipitates increased gradually. The solidus temperatures andγ′ precipitates morphology of four Co-Al-W base alloys are nearly unchanged. When the nickel content in Co-8.8Al-9.8W alloy reaches 25%γ′ precipitates transformation temperatures increased to 1100℃. The typical of γ/γ′ two-phase micro-structure is generated in four alloys after the heat treatment at 900 ℃ for 50 h. When prolonged aging at 900 ℃ for 100 h , the γ′ precipitates volume fraction decreases to different degree and there is an obvious phenomenon of the γ′ precipitates become coarsen as a function of Ni concentration . The microhardness results of the four alloys after heat treatment at 900 ℃ for 50 h and 100 h indicate that the microhardness is risen from 5Ni to 15Ni alloy, lowered in alloys with higher Ni content. With the aging treatment time prolonged from 50h to 100h, the microhardness of alloys becomes small.

    参考文献
    相似文献
    引证文献
引用本文

徐仰涛,夏荣里,娄德超.镍含量对Co-8.8Al-9.8W基合金时效组织演变与γ′相溶解行为的影响[J].稀有金属材料与工程,2017,46(8):2288~2293.[Xu Yangtao, XiaRongli, Lou Dechao. Effects of Nickel Content on Microstructural Evolution and γ′ Dissolution of Co-8.8Al-9.8W Base Alloys[J]. Rare Metal Materials and Engineering,2017,46(8):2288~2293.]
DOI:[doi]

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2016-01-12
  • 最后修改日期:2016-03-13
  • 录用日期:2016-03-30
  • 在线发布日期: 2017-11-16
  • 出版日期: