The Microstructure and Electrochemical Behavior of AZ91-3Ca Magnesium Alloy
Author:
Affiliation:

University of Science and Technology Liaoning,University of Science and Technology Liaoning,University of Science and Technology Liaoning,University of Science and Technology Liaoning,University of Science and Technology Liaoning

Fund Project:

The National Natural Science Foundation of China (General Program, Key Program, Major Research Plan);University of Science and Technology Liaoning graduate education reform and science and technology innovation and Entrepreneurship Project

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    利用扫描电镜(SEM)、X射线衍射仪(XRD)以及电化学测试法和失重法研究了铸态AZ91-3Ca镁合金分别退火处理前后的相组成以及不同退火处理条件下的腐蚀性为。结果表明,铸态AZ91-3Ca镁合金主要由基体α-Mg相和沿着晶界附近分布的网状共晶相组成。共晶相中含有α-Mg相,实心块状β-Mg17Al12相和网状(Mg,Al)2Ca等相。300℃和400℃退火处理后合金的组织结构没有明显变化,但是在较高退火温度500℃下保温2.0 h后,β-Mg17Al12相溶解促进了一种含有Mg,Al,Zn,Ca四种元素的四元相的生成。在500℃保温16.0 h 后,基体中Al元素含量最多,且分布均匀,在NaCl水溶液中耐蚀性能最佳,其自腐蚀电位为-1330mV,电流密度为1.222×10-4 A/cm2,腐蚀速率为0.11mg/cm2h。

    Abstract:

    The microstructure of as-cast AZ91-3Ca magnesium alloy before and after annealing treatment and the corrosion behavior under different annealing conditions were studied by scanning electron microscopy (SEM), X-ray diffractometer (XRD), electrochemical test and weight loss method. The results show that the as cast AZ91-3Ca alloy is mainly composed of matrix a -Mg phase and a network eutectic phase along the grain boundaries. The eutectic phase contains a -Mg phase, a solid block β-Mg17Al12 phase and a Mg (Al) 2Ca phase. The microstructures of the alloys annealed at 300 ℃ and 400 ℃ have no obvious change. After annealing at 500 ℃ for 2.0 h, the solution of β-Mg17Al12 phase promotes the precipitation of Mg, Al, Zn and Ca new phase. After annealing at 500 ℃ for 16.0 h, the content of Al in the matrix is the most, and the distribution is uniform and the corrosion resistance is the best, in NaCl aqueous solution the corrosion potential was -1330 mV, the current density was 1.222 × 10-4 A / cm2, and the corrosion rate was 0.11 mg / cm2h.

    参考文献
    相似文献
    引证文献
引用本文

王冬晓,王忠军,张涛,褚旭,王洪斌. AZ91-3Ca镁合金组织结构和电化学行为的研究[J].稀有金属材料与工程,2018,47(9):2735~2742.[Wang Dongxiao, Wang Zhongjun, Zhang Tao, Chu Xu, Wang Hongbin. The Microstructure and Electrochemical Behavior of AZ91-3Ca Magnesium Alloy[J]. Rare Metal Materials and Engineering,2018,47(9):2735~2742.]
DOI:[doi]

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2016-10-10
  • 最后修改日期:2017-04-13
  • 录用日期:2017-04-13
  • 在线发布日期: 2018-11-01
  • 出版日期: