Effect on Structure and Properties of Finemet-type Ribbon by Collaboratively Adjusting Nb, Si, B
Author:
Affiliation:

1.School of Materials Science and Engineering,Hebei University of Technology;2.Tian Jin Sun Hope New Energy Technology co,Ltd,Tianjin

Fund Project:

National Natural Science Foundation of China (Project No. 51671078,51271072), National Natural Science Youth Foundation(51301056), Natural Science of Hebei Province (E2015202008)

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    本文用V部分替代Nb并适当调整Si与B的含量,通过单辊快淬技术及退火工艺制备了原始成分为Fe73Si15Nb3B8Cu1和优化成分为Fe73Si15.5Nb1.1V2.4B7Cu1的Finemet型非晶纳米晶薄带。利用X射线衍射仪、透射电子显微镜、磁性能测试仪研究了薄带的结构及磁性能。结果表明:两种快淬态薄带主要为非晶结构,合金具有良好的非晶形成能力;采用Luborsky法评价薄带韧性,发现含V的快淬态薄带的断裂应变λt为5.05×10-2,其韧性较差;两种退火态薄带中的纳米晶晶粒大小分别约为14.8 nm与13.2 nm;与原始成分薄带相比,含V薄带的居里温度Tc,晶化起始温度Tx1有少量降低;含V薄带的饱和磁化强度略低于原始薄带,但是其矫顽力较小,其环形磁芯样品静态初始磁导率为1.269×105、静态损耗为1.748 J/m3,动态测试显示,随着频率的增加,含V薄带损耗较原始薄带小的优势更加明显。

    Abstract:

    In this paper, the Finemet-type amorphous-nanocrystalline ribbons with original Fe73Si15Nb3B8Cu1 and optimized composition Fe73Si15.5Nb1.1V2.4B7Cu1 substituted partial Nb for V as well as appropriately adjusted Si and B were prepared by single-roller rapid quenching and isothermal annealing technology. The microstructure and magnetic properties of the ribbons were studied by X ray diffraction, transmission electron microscopy and magnetic performance testers. The results show that two types of as-spun ribbons are mainly composed of amorphous phase, meaning that two kinds of alloys have good amorphous forming ability; According to Luborsky principle, the fracture srain λt is 5.05×10-2, which indicates that the toughness is poor; The nanocrystalline grain size of two kinds of annealed ribbons are 14.8 nm and 13.2 nm, respectively; Compared with the original composition ribbons,Curie temperature Tc and first crystallization temperature Tx1 of V-containing ribbons are slightly decreased; While the saturation magnetization of the V-containing ribbon is slightly lower than that of the V-free ribbon, the coercivity is smaller, initial permeability and static loss of the ring-shaped V-containing magnetic core samples reach 1.269×105 and 1.748 J/m3 respectively, and their AC iron loss advantage is more and more obvious than that of V-free ones with increasing frequency.

    参考文献
    相似文献
    引证文献
引用本文

杜帅龙,张策,边璐鹏,孙继兵,张 磊,步绍静. Nb、Si、B含量的联动调整对Finemet型薄带结构及性能的影响[J].稀有金属材料与工程,2018,47(11):3548~3553.[Du shuailong, Zhang Ce, Bian Lupeng, Sun Jibing, Zhang Lei, Bu shaojing. Effect on Structure and Properties of Finemet-type Ribbon by Collaboratively Adjusting Nb, Si, B[J]. Rare Metal Materials and Engineering,2018,47(11):3548~3553.]
DOI:[doi]

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2017-03-14
  • 最后修改日期:2018-11-16
  • 录用日期:2017-06-23
  • 在线发布日期: 2018-12-19
  • 出版日期: