+高级检索
奥氏体系合金激光焊接凝固裂纹敏感性研究
作者:
作者单位:

1.江苏大学;2.大阪大学, 日本 大阪府;3.广岛大学,日本 广岛县东广岛市;4.国立技术研究所吴校区, 日本 广岛县吴市

作者简介:

通讯作者:

中图分类号:

基金项目:

国家自然科学基金(51705219)、江苏大学高级人才科研启动基金(17JDG039)


Study on Solidification Cracking Susceptibility of Austenitic Alloys during Laser Welding
Author:
Affiliation:

1.Jiangsu University;2.Osaka University;3.Hiroshima University;4.National Institute of Technology, Kure College

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    本文基于舍弗勒相图系统研究了奥氏体系合金激光焊接凝固裂纹敏感性。利用激光热丝焊工艺制备了含不同化学成分镍基焊丝的焊接接头,借助横向可调拘束实验和温度测量获得了脆性温度区间,对凝固裂纹敏感性进行定量评估。结果表明,铬镍当量之比(Creq / Nieq)在0.1 ~ 1.2之间时,脆性温度区间呈现出先增加后下降的趋势,说明凝固裂纹敏感性随着Creq / Nieq值的增加先增加再降低。在舍弗勒相图单相奥氏体区域内,中间区域敏感性相对较高,周边区域敏感性相对较低。这是因为焊缝中P + S、Nb和Si等合金元素含量增加,可促使形成低熔点共晶化合物-偏析液膜,导致凝固裂纹敏感性增加。另外,在一定条件下,Nb对凝固裂纹敏感性的影响要远大于P + S等的影响。

    Abstract:

    Based on the Schaeffler diagram, the solidification cracking susceptibility of austenitic alloys during laser welding was investigated systematically. Specimens with different chemical compositions were made up by laser welding with hot different Nickel-based wires. Brittleness temperature range (BTR) could be obtained by combining the result of solidification crack from laser Trans-Varestraint test with the temperature profile of weld bead during laser welding. Then the solidification cracking susceptibility was studied quantitatively using BTR. With the increase of the ratio of Cr equivalent to Ni equivalent (Creq / Nieq) from 0.1 to 1.2, the BTR tended to increase firstly and then decrease. This showed that the solidification cracking susceptibility had a tendency of increasing and decreasing with increasing Creq / Nieq. While, the solidification cracking susceptibility was relatively higher in the middle region, and the susceptibility was lower at the sides of the single phase austenite region in the single phase austenite region of the Schaeffler diagram. When the contents of P + S, Nb and Si alloy elements were relatively higher, the low melting point eutectic compound – segregated liquid film could be formed at the grain boundary and sub-grain boundary, leading to increase the solidification cracking susceptibility. In addition, the effect of Nb on the solidification cracking susceptibility was much higher than that of P + S under a certain condition.

    参考文献
    相似文献
    引证文献
引用本文

王丹,门井浩太,山本元道,篠崎贤二.奥氏体系合金激光焊接凝固裂纹敏感性研究[J].稀有金属材料与工程,2021,50(7):2435~2446.[Wang Dan, Kadoi Kota, Yamamoto Motomichi, Shinozaki Kenji. Study on Solidification Cracking Susceptibility of Austenitic Alloys during Laser Welding[J]. Rare Metal Materials and Engineering,2021,50(7):2435~2446.]
DOI:10.12442/j. issn.1002-185X.20200560

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2020-08-01
  • 最后修改日期:2020-09-21
  • 录用日期:2020-10-15
  • 在线发布日期: 2021-08-09
  • 出版日期: 2021-07-31