GH4169合金不同孔形气膜冷却孔疲劳性能对比分析
作者:
作者单位:

1.四川大学 空天科学与工程学院;2.北京卫星环境工程研究所;3.清华大学航空发动机研究院,北京

作者简介:

通讯作者:

中图分类号:

TG113.25+5

基金项目:

航天创新基金(CAST-BISEE2019-017)


Fatigue Property Investigation of GH4169 Alloy Film Cooling Holes with Different Shapes
Author:
Affiliation:

1.School of Aeronautics and Astronautics,Sichuan University;2.Institute of Aero Engine,Tsinghua University,Beijing ,China

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    气膜冷却孔是航空航天高温部件常见冷却设计,但属于典型结构疲劳危险点。为了优化气膜冷却孔热-机械性能,本文通过疲劳试验和有限元建模分析,研究GH4169合金相同底孔尺寸下的气膜冷却孔疲劳性能。研究表明:相同底孔直径下,90°圆孔疲劳寿命远低于倾斜圆孔、扇形孔和扇形后倾孔;相同孔倾角下,孔形对疲劳寿命影响较小;90°圆孔发生单断口疲劳断裂,断口与加载方向基本垂直,而倾斜圆孔、扇形孔、扇形后倾孔在孔根部附近发生疲劳断裂,断口向孔轴方向倾斜,除主断口外在孔根部均出现亚断口;90°圆孔断口疲劳裂纹在孔壁中间萌生,而倾斜圆孔和扇形孔疲劳裂纹在孔口部位萌生,且呈现多源萌生特征;裂纹萌生区平整光滑,随着裂纹扩展断口表面韧窝明显增多;孔轴倾角和孔口形状对孔周应力分布及最大应力水平具有显著影响。

    Abstract:

    Film cooling is a common cooling design in aerospace high temperature components, and it is also a typical fatigue risk point of the whole structure. To optimize designs of film cooling holes, an experimental and numerical study was conducted to investigatred fatigue properties of GH4169 alloy film cooling holes with different shapes. Results showed that the fatigue life of the circular shaped hole was obviously lower than those of both the oval shaped hole and the dust-pan shaped hole, and the hole shape exhibited a few influence on the fatigue life of the specimens corresponding to the same skew angle of holes. The specimens of the circular shaped hole failed with only one fracture surface, and the fracture surface was perpendicular to the loading direction. However, the specimens of the oval shaped hole and the dust-pan shaped hole failed with master fracture surface and slave master fracture surface, and the fracture surface was along the hole axis direction. Fatigue crack initiation occurred at the middle region of the circular shaped hole, while fatigue crack initiation occurred at both the entrance and the exit of the oval shaped and the dust-pan shaped hole. The crack initiation zone was flat and smooth, moreover, more dimples were observed on the fracture surface with fatigue crack propagating. Both the skew angle of holes and the shape hole orifice exhibited significant influence on the tress distribution and the peak stress of the hole under quasi-static loading.

    参考文献
    相似文献
    引证文献
引用本文

左杨杰,杨艳静,陈伟,徐全勇. GH4169合金不同孔形气膜冷却孔疲劳性能对比分析[J].稀有金属材料与工程,2022,51(6):2224~2230.[Zuo Yangjie, Yang Yanjing, Chen Wei, Xu Quanyong. Fatigue Property Investigation of GH4169 Alloy Film Cooling Holes with Different Shapes[J]. Rare Metal Materials and Engineering,2022,51(6):2224~2230.]
DOI:10.12442/j. issn.1002-185X.20210509

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2021-06-10
  • 最后修改日期:2021-07-23
  • 录用日期:2021-08-06
  • 在线发布日期: 2022-07-06
  • 出版日期: 2022-06-29