+高级检索
碳载PtNi合金催化剂的制备、表征及氧还原催化性能研究
作者:
作者单位:

昆明贵金属研究所 稀贵金属综合利用新技术国家重点实验室

作者简介:

通讯作者:

中图分类号:

基金项目:

国家自然科学基金(项目号:51864022);昆明市高层次人才引进创新技术进步项目(项目号:13020163);云南贵金属集团R D应用研究(2020040603)


Preparation, Characterization and Oxygen Reduction Reaction Catalytic Performance of Carbon Loaded PtNi Alloy Catalysts
Author:
Affiliation:

1.Kunming Institute of Precious Metals,State Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals Kunming 650106;2.China

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    以乙酰丙酮铂(Pt(acac)2)、乙酰丙酮镍(Ni(acac)2)为前驱体,三正辛基氧膦(TOPO)为表面修饰剂,油胺(OAm)为还原剂,N,N-二甲基甲酰胺(DMF)为助剂,超导碳科琴黑ECP为载体,采用液相合成法制备了碳载PtNi合金纳米催化剂(Pt2.7Ni/C)。通过TEM对其形貌进行表征,ICP-AES进行定性和定量分析,XRD对其结构进行表征,并进行电化学阴极氧还原催化性能研究。研究表明:所制备的Pt2.7Ni/C纳米催化剂粒径分布在3~11 nm之间,平均粒径为6.25 nm;在酸性条件下,当电位在0.9 V(vs. RHE)时,Pt2.7Ni/C纳米催化剂的质量比活性为796.08 mA mg-1Pt,为商业Pt/C(JM)催化剂的4.0倍,面积比活性为3.60 mA cm-2,为商业Pt/C(JM)催化剂的11.3倍。同时在经过5000和10000圈的加速耐久性实验后,Pt2.7Ni/C纳米催化剂催化活性依旧高于商用Pt/C(JM)催化剂,表现出优异的氧还原催化性能。

    Abstract:

    Carbon loaded PtNi alloy nanocatalysts (Pt2.7Ni/C) were prepared by liquid phase synthesis using platinum acetylacetonate (Pt(acac)2) and nickel acetylacetonate (Ni(acac)2) as precursors, tri-n-octylphosphine oxide (TOPO) as surface modifier, oleylamine (OAm) as reducing agent, N,N-dimethylformamide (DMF) as auxiliary, and superconducting carbon kochen black ECP as carrier. The morphology of Pt2.7Ni/C was characterized by TEM, the qualitative and quantitative analysis by ICP-AES, the structural characterization by XRD, and the electrochemical cathodic oxygen reduction catalytic performance was further investigated. It was shown that the particle size of the prepared Pt2.7Ni/C nanocatalysts were in range of 3-11 nm with an average size of ~6.25 nm. The mass activity of Pt2.7Ni/C nanocatalysts was 796.08 mA.mg-1Pt (4.0 times as effective as the commercial Pt/C(JM) catalysts) and the specific activity was 3.60 mA.cm2(11.3 times as effective as the commercial Pt/C(JM) catalysts) under acidic conditions when the potential was at 0.9 V (vs. RHE). The catalytic activity of the Pt2.7Ni/C nanocatalysts remained higher than that of the commercial Pt/C(JM) catalysts after 5000 and 10000 turns of accelerated endurance experiments, showing excellent oxygen reduction catalytic performance of the Pt2.7Ni/C nanocatalysts.

    参考文献
    相似文献
    引证文献
引用本文

李鸿鹏,蒋云波,何建云.碳载PtNi合金催化剂的制备、表征及氧还原催化性能研究[J].稀有金属材料与工程,2023,52(4):1345~1351.[Li Hongpeng, Jiang Yunbo, He Jianyun. Preparation, Characterization and Oxygen Reduction Reaction Catalytic Performance of Carbon Loaded PtNi Alloy Catalysts[J]. Rare Metal Materials and Engineering,2023,52(4):1345~1351.]
DOI:10.12442/j. issn.1002-185X.20220278

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2022-04-06
  • 最后修改日期:2022-05-20
  • 录用日期:2022-05-25
  • 在线发布日期: 2023-05-01
  • 出版日期: 2023-04-25