Cr3C2含量对Ni3Al基合金激光熔覆层组织与性能的影响
作者:
作者单位:

1.钢铁研究总院有限公司焊接研究所;2.查尔姆斯理工大学,哥德堡 SE-

作者简介:

通讯作者:

中图分类号:

基金项目:

国家重点研发计划(2020YFE0200900)钢铁研究总院自主投入研发专项项目(事23H60440ZD)


Effect of Cr3C2 content on microstructure and properties in laser cladding of Ni3Al based alloy
Author:
Affiliation:

1.Welding Institute,Central Iron and Steel Research Institute;2.Chalmers University of Technology,Goteborg SE- ,Sweden

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    本文借助激光熔覆技术,在45钢上开展不同Cr3C2添加量的Ni3Al+Cr3C2混合粉末制备Ni3Al基合金激光熔覆层试验研究,利用扫描电镜、X射线衍射仪、透射电镜及摩擦磨损试验机等设备,统计不同Cr3C2添加量下原位自生碳化物的含量及尺寸,分析碳化物对Ni3Al基合金熔覆层显微组织、显微硬度及摩擦磨损性能的影响。结果表明:Ni3Al基合金激光熔覆层组织主要为Ni3Al基相和原位自生的Cr7C3碳化物。随着Cr3C2含量的增加,熔覆层原位自生碳化物含量由6.8%增加至32.3%,平均尺寸由0.10 μm增长至0.78 μm,熔覆层显微硬度由471HV提高至609HV。当Cr3C2含量为35%时,碳化物呈小颗粒弥散分布,摩擦磨损过程中产生均匀磨损,使熔覆层磨损量低至0.19 mg,此时对磨盘的磨损量相对最低,约为1.23 mg;而当Cr3C2含量为45%时,碳化物含量虽然达到32.3%,但多以大尺寸颗粒为主,在摩擦磨损过程中大颗粒碳化物发生断裂剥落,加速了对磨盘的磨损。

    Abstract:

    Using Ni3Al+Cr3C2 mixed powder with different amounts of Cr3C2, laser cladding was carried out on 45 steel to prepare Ni3Al-based alloy cladding layer. By means of scanning electron microscopy (SEM), X-ray diffraction (XRD), transmission electron microscopy (TEM), and wear tests, the content and average size of in situ-formed carbides under different amounts of Cr3C2 were calculated, and the effects of carbides on the microstructure, microhardness and wear resistance of Ni3Al-based alloy cladding layer were analyzed. The results indicate that the microstructure of the Ni3Al-based alloy cladding layer contains mainly Ni3Al matrix and in situ-formed Cr7C3 carbides. With the increase of Cr3C2 content, the proportion of in situ-formed carbides in cladding layer increases from 6.8% to 32.3%, the average size increases from 0.10μm to 0.78μm, and the microhardness of the cladding layer increases from 471HV to 609HV. When the content of Cr3C2 is 35%, the carbide particles are dispersed, and uniform wear is produced in the process of wear test, so that the wear less of cladding layer is as low as 0.19 mg, and the wear loss of the disk is relatively the lowest, about 1.23 mg. However, when the content of Cr3C2 is 45%, the carbide content is 32.3%, but the large size particles are mainly. In the process of wear test, the large particles of carbide fracture and spalling, which accelerates the wear of the disk.

    参考文献
    相似文献
    引证文献
引用本文

阚成玲,彭云,龚侠,李长海,赵琳,田志凌. Cr3C2含量对Ni3Al基合金激光熔覆层组织与性能的影响[J].稀有金属材料与工程,2024,53(10):2852~2859.[Chengling Kan, Yun Peng, Karin Gong, Changhai Li, Lin Zhao, Zhiling Tian. Effect of Cr3C2 content on microstructure and properties in laser cladding of Ni3Al based alloy[J]. Rare Metal Materials and Engineering,2024,53(10):2852~2859.]
DOI:10.12442/j. issn.1002-185X.20230511

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2023-08-18
  • 最后修改日期:2023-10-19
  • 录用日期:2023-11-13
  • 在线发布日期: 2024-10-17
  • 出版日期: 2024-09-27