Cr2O3涂层对硅基陶瓷型芯与镍基单晶高温合金润湿性及界面反应的影响
作者:
作者单位:

1.中国科学院金属研究所 师昌绪先进材料创新中心,辽宁 沈阳 110016;2.中国科学技术大学 材料科学与工程学院,辽宁 沈阳 110016;3.空装驻沈阳地区第三军事代表室,辽宁 沈阳 110144

作者简介:

通讯作者:

中图分类号:

TG174.444;TG132.3+3

基金项目:

国家重点研发计划(2017YFA0700704,2019YFA0705300);四川省科技计划(省院省校合作项目)(2022YFSY0016);辽宁省优秀青年基金(2021-YQ-02)


Effect of Cr2O3 Coating on Wettability and Interfacial Reaction Between Silicon-Based Ceramic Core and Nickel-Based Single Crystal Superalloy
Author:
Affiliation:

1.Shi-changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China;2.School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China;3.Third Military Representative Room in Shenyang Area Air Force Equipment, Shenyang 110144, China

Fund Project:

国家重点研发计划(项目号No.2017YFA0700704和2019YFA0705300);四川省科技计划项目(省院省校合作项目)(项目号No.2022YFSY0016);辽宁省优秀青年基金(项目号No. 2021-YQ-02)

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    通过多弧离子镀法在硅基陶瓷型芯表面制备Cr2O3涂层,借助高温原位座滴法实验研究了Cr2O3涂层对硅基陶瓷型芯与镍基单晶高温合金在1550 ℃接触后的润湿行为以及界面反应行为的影响,并利用SEM、EDS和XRD对界面反应后的界面形貌、元素分布以及反应产物进行了分析。研究发现,镍基单晶高温合金在涂覆Cr2O3涂层的硅基陶瓷型芯上的润湿角为98.29°。高温合金熔体中Hf、Al与Cr2O3涂层反应,在高温合金底部生成HfO2、Al2O3以及游离的Cr。生成的Al2O3形成保护层阻止高温合金中活泼元素向界面扩散,但仍有少量高温合金熔体与失去涂层保护的硅基陶瓷基体发生反应,在界面处生成Al2O3以及游离的Si。生成的Cr、Si在界面处富集并在高温合金表面生成CrSi2;部分Si自高温合金表面向内部扩散,与W等难熔元素在高温合金近表面处形成(Mo,W,Re)5Si3。结果表明,镍基单晶高温合金在涂覆Cr2O3涂层的硅基陶瓷型芯上的润湿角相较于在未表面改性的硅基陶瓷型芯上的润湿角小,润湿性好。综合上述分析,在硅基型芯表面涂覆Cr2O3涂层有利于改善铸件局部位置的合金充型,但对界面反应控制效果有限。

    Abstract:

    This research applied Cr2O3 coating on the surface of silicon-based ceramic core through multi-arc ion plating method. The effect of Cr2O3 coating on wetting behavior and interface reaction behavior of silicon-based ceramic core and nickel-based single crystal superalloy after contact at 1550 ℃ were studied using high-temperature in-situ droplet method. The interface morphology, element distribution, and reaction products after the interface reaction were analyzed using SEM, EDS, and XRD. The results show that the wetting angle between nickel-based single crystal superalloy and silicon-based ceramic core coated with Cr2O3 is 98.29°. Hf and Al in superalloy melt react with Cr2O3 coating, generating HfO2, Al2O3, and free Cr at the bottom of superalloy. The generated Al2O3 forms a protective layer to prevent the diffusion of active elements in superalloy to the interface. However, a small amount of superalloy melt still reacts with the silicon-based ceramic substrate without coating protection, generating Al2O3 and free Si at the interface. The generated Cr and Si are enriched at the interface and form CrSi2 on the superalloy surface. Part of Si diffuses from the surface of the superalloy to the interior, forming (Mo,W,Re)5Si3 with refractory elements such as W near the surface of superalloy. The results indicate that the wetting angle of nickel-based single crystal superalloy on silicon-based ceramic core coated with Cr2O3 is smaller than that on unmodified silicon-based ceramic cores, and its wettability is better. Based on the above analyses, the Cr2O3 coating on the surface of silicon-based cores is beneficial to improve the filling of alloy at local positions of castings, but its control effect on interface reactions is limited.

    参考文献
    相似文献
    引证文献
引用本文

何家宝,王亮,邹明科,张朝威,王新广,姜肃猛,吴佳欣,孟杰,周亦胄.Cr2O3涂层对硅基陶瓷型芯与镍基单晶高温合金润湿性及界面反应的影响[J].稀有金属材料与工程,2025,54(1):202~208.[He Jiabao, Wang Liang, Zou Mingke, Zhang Chaowei, Wang Xinguang, Jiang Sumeng, Wu Jiaxin, Meng Jie, Zhou Yizhou. Effect of Cr2O3 Coating on Wettability and Interfacial Reaction Between Silicon-Based Ceramic Core and Nickel-Based Single Crystal Superalloy[J]. Rare Metal Materials and Engineering,2025,54(1):202~208.]
DOI:10.12442/j. issn.1002-185X.20230706

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2023-11-08
  • 最后修改日期:2023-11-26
  • 录用日期:2023-12-18
  • 在线发布日期: 2025-01-24
  • 出版日期: 2025-01-20