+高级检索
热处理对选区激光熔化成形大层厚Ti-6Al-4V钛合金的影响
作者:
作者单位:

1.昆明理工大学 机电工程学院,云南 昆明 650500;2.昆明理工大学 材料科学与工程学院,云南 昆明 650093

作者简介:

通讯作者:

中图分类号:

TG146.23;TG166.5

基金项目:

云南省“兴滇英才支持计划”项目(KKRD202201090);云南省重大科技专项(202202AG050007);云南省重点研发项目(202103AN080001-002);云南省基础研究计划(202101AS070017)


Effect of Heat Treatment on Selective Laser Melting Formed Ti-6Al-4V Titanium Alloy with High Layer Thickness
Author:
Affiliation:

1.Faculty of Mechanical and Electrical Engineering, Kunming University of Science and Technology, Kunming 650500, China;2.School of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    增加铺粉厚度可以明显提高选区激光熔化(selective laser melting,SLM)技术制备Ti-6Al-4V的效率,但其成形质量相比于常规层厚较差。退火热处理可以提高选区激光熔化制备钛合金试样的延展性,但其对大层厚成形钛合金的影响仍不明确。本实验利用选区激光熔化技术制备大层厚Ti-6Al-4V,随后在700和950 ℃退火处理,研究退火处理对Ti-6Al-4V组织性能的影响。研究表明,制备的大层厚钛合金在扫描速度600~800 mm/s时可以取得较好的成形质量。热处理后试样的微观组织由针状马氏体逐渐变粗随后转变为板条状,在950 ℃热处理后试样的XRD衍射峰中观察到β峰,这会影响材料的压缩性能。其中扫描速度为600 mm/s时制备的试样抗压强度为1593 MPa,最大断裂应变为15.1%;退火热处理后抗压强度降低到1359 MPa,最大断裂应变提升到22.2%,断裂形式从脆性断裂转变为韧性-脆性断裂。

    Abstract:

    Increasing the layer thickness can significantly improve the preparation efficiency of selecting laser melting formed Ti-6Al-4V. However, it leads to lower forming quality in comparison to the alloy with low layer thickness. Annealing heat treatment can improve the ductility of titanium alloy prepared by selective laser melting, but the effect of annealing heat treatment on the sample with high layer thickness is not clear. In this research, the Ti-6Al-4V with high layer thickness was fabricated by selective laser melting. The 700 and 950 ℃ were set as annealing heat treatment temperatures, and the effects of heat treatment on the microstructure and properties of Ti-6Al-4V were investigated. The results reveal that the preparation of samples can achieve good forming quality when the scanning speed ranges from 600 mm/s to 800 mm/s. After annealing at 700 and 950 ℃, the microstructure of the samples transforms from acicular martensite to lath martensite. The β phase can be observed after heat treatment at 950 ℃. The changes in compression performance are influenced by the microstructure. The ultimate compressive strength of the prepared sample with a scanning speed of 600 mm/s is 1593 MPa, and the maximum fracture strain is 15.1%. After annealing heat treatment, the ultimate compressive strength decreases to 1359 MPa and the maximum fracture strain increases to 22.2%. The fracture mode changes from brittle fracture to ductile-brittle fracture.

    参考文献
    相似文献
    引证文献
引用本文

姚碧波,彭钰洋,黎振华,刘美红,李海,王丛.热处理对选区激光熔化成形大层厚Ti-6Al-4V钛合金的影响[J].稀有金属材料与工程,2025,54(5):1235~1244.[Yao Bibo, Peng Yuyang, Li Zhenhua, Liu Meihong, Li Hai, Wang Cong. Effect of Heat Treatment on Selective Laser Melting Formed Ti-6Al-4V Titanium Alloy with High Layer Thickness[J]. Rare Metal Materials and Engineering,2025,54(5):1235~1244.]
DOI:10.12442/j. issn.1002-185X.20230818

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2023-12-19
  • 最后修改日期:2024-01-12
  • 录用日期:2024-02-01
  • 在线发布日期: 2025-05-23
  • 出版日期: 2025-05-22