+高级检索
时效处理对Ti-3Al-6Mo-2Fe-2Zr激光焊接接头组织和性能的影响
DOI:
作者:
作者单位:

河海大学 材料科学与工程学院,江苏 常州 213022

作者简介:

通讯作者:

中图分类号:

基金项目:

NSFC(51804097), Fundamental Research Funds for the Central Universities of China (B220202026), Changzhou Sci&Tech Program (CJ20220074)


Influence of Aging Treatment on Microstructure and Pro-perties of Ti-3Al-6Mo-2Fe-2Zr Laser-Welded Joint
Author:
Affiliation:

College of Materials Science and Engineering, Hohai University, Changzhou 213022, China

Fund Project:

National Natural Science Foundation of China (51804097); Fundamental Research Funds for the Central Universities of China (B220202026); Changzhou Sci&Tech Program (CJ20220074)

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    采用激光焊接近β钛合金(Ti-3Al-6Mo-2Fe-2Zr),并对激光焊接接头进行不同温度的时效处理,揭示了时效温度、显微组织和接头拉伸性能之间的关系。结果表明,由于该合金具有较高的Mo当量且激光焊接时冷却速度较快,焊缝主要由单一β相组成。时效处理后,在焊缝和热影响区中析出了大量的α相,随着时效温度的升高,α相粗化,体积分数降低。与焊态接头相比,时效处理后接头的抗拉伸强度和延伸率均有提升。但随时效温度的升高,α相的体积分数减少,强化效果减弱。当合金在500 ℃时效8 h时,接头获得了最佳的强度和塑性匹配。接头的断裂模式由焊态下的准解理断裂转变为时效处理后的微孔聚集型断裂。

    Abstract:

    Laser beam welding was used to join a near-β titanium alloy (Ti-3Al-6Mo-2Fe-2Zr), followed by aging treatments. The relations among aging temperature, microstructure, and tensile properties of joints were revealed. For as-welded joints, the fusion zone features primarily single β phase. It is attributed to the high Mo equivalency of this alloy and the fast cooling rate in laser beam welding. After aging treatments, many α precipitates form in the fusion zone and heat affected zone. The rising aging temperature coarsens α precipitates and reduces the volume fraction of α precipitates. Compared with the as-welded joints, the aging treated joints'' tensile strength and elongation are improved. The increasing aging temperature weakens the strengthening effect because of the decreasing volume fraction of α precipitates. After the aging treatment at 500 °C for 8 h, the joints obtain the optimal match between strength and plasticity. The fracture mode of joints changes from quasi-cleavage fracture in as-welded condition to microvoid coalescence fracture after heat treatments.

    参考文献
    相似文献
    引证文献
引用本文

万轩,何超威,张可召,刘栋,严春妍,包晔峰.时效处理对Ti-3Al-6Mo-2Fe-2Zr激光焊接接头组织和性能的影响[J].稀有金属材料与工程,2025,54(4):930~936.[Wan Xuan, He Chaowei, Zhang Kezhao, Liu Dong, Yan Chunyan, Bao Yefeng. Influence of Aging Treatment on Microstructure and Pro-perties of Ti-3Al-6Mo-2Fe-2Zr Laser-Welded Joint[J]. Rare Metal Materials and Engineering,2025,54(4):930~936.]
DOI:[doi]

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2024-03-01
  • 最后修改日期:2025-03-22
  • 录用日期:2024-05-07
  • 在线发布日期: 2025-04-23
  • 出版日期: 2025-04-21