Kinetics and Characteristics of Isothermal Constant Volume Hydrogen Desorption in TC21 Alloy
Author:
Affiliation:

School of Materials Science and Engineering, Hefei University of Technology, Hefei 230009, China

Fund Project:

National Natural Science Foundation of China (52275328, 51875157)

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    使用定容法研究了TC21合金放氢的动力学及特性、剩余氢含量和激活能。结果表明,放氢温度和初始氢压影响TC21合金的放氢特性。当氢化TC21合金在700~940 ℃温度范围内放氢时,放氢过程主要由形核长大过程(kt=[-ln(1-α)]2/3)、化学反应过程(kt= (1-α)-1/2)和三维扩散过程(kt=[1-(1-α)1/3]1/2)控制。当氢化TC21合金放氢时,各过程的速率常数之间存在以下关系:k(化学反应过程)> k(形核长大过程)> k(三维扩散过程)。氢化TC21合金放氢后的剩余氢含量随着放氢温度的升高而逐渐减少,随着初始氢压的升高而逐渐增加。TC21合金在放氢过程中的激活能约为26.663 kJ/mol。

    Abstract:

    Hydrogen desorption kinetics and characteristics, residual hydrogen content and activation energy of TC21 alloy were investigated by the constant volume method. Results show that hydrogen desorption temperature and initial hydrogen pressure affect hydrogen desorption characteristics of TC21 alloy. The hydrogen desorption process is mainly dominated by nucleation and growth process (kt=[-ln(1-α)]2/3), chemical reaction process (kt=(1-α)-1/2) and three-dimensional diffusion process (kt=[1-(1-α)1/3]1/2) when the hydrogenated TC21 alloy is dehydrogenated at temperatures of 700–940 °C. When the hydrogenated TC21 alloy releases hydrogen, the following relationship exists among the rate constants of each process: k (chemical reaction process)>k (nucleation and growth process)>k (three-dimensional diffusion process). The residual hydrogen content of the hydrogenated TC21 alloy after hydrogen desorption decreases gradually with the increase in hydrogen desorption temperature, and increases gradually with the increase in the initial hydrogen pressure. The activation energy of TC21 alloy in the process of hydrogen desorption is about 26.663 kJ/mol.

    参考文献
    相似文献
    引证文献
引用本文

袁宝国,栾海波,万伟,田翔,陈牧,陈帅,苏纯绅.TC21合金等温定容放氢动力学及特性[J].稀有金属材料与工程,2025,54(7):1697~1705.[Yuan Baoguo, Luan Haibo, Wan Wei, Tian Xiang, Chen Mu, Chen Shuai, Su Chunshen. Kinetics and Characteristics of Isothermal Constant Volume Hydrogen Desorption in TC21 Alloy[J]. Rare Metal Materials and Engineering,2025,54(7):1697~1705.]
DOI:10.12442/j. issn.1002-185X.20240289

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2024-05-15
  • 最后修改日期:2024-08-17
  • 录用日期:2024-08-19
  • 在线发布日期: 2025-07-01
  • 出版日期: 2025-06-23