+高级检索
放电等离子烧结WMoNbTaV-Al2O3 高熵合金组织及磨损性能
作者:
作者单位:

1.河南科技大学 材料科学与工程学院,河南 洛阳 471000;2.河南科技大学 河南省高温难熔金属材料国际联合实验室,河南 洛阳 471000;3.中国工程物理研究院 核物理与化学研究所,四川 绵阳 621900

作者简介:

通讯作者:

中图分类号:

基金项目:

NSFC(U2004180); National Key R&D Program of China(2020YFB2008400)


Microstructure and Wear Properties of WMoNbTaV-Al2O3 High Entropy Alloy Prepared by Spark Plasma Sintering
Author:
Affiliation:

1.School of Materials Science and Engineering, Henan University of Science and Technology, Luoyang 471000, China;2.Henan International Joint Laboratory for High Temperature Refractory Metal Materials, Henan University of Science and Technology, Luoyang 471000, China;3.Institute of Nuclear Physics and Chemistry, China Academy of Engineering Physics, Mianyang 621900, China

Fund Project:

National Natural Science Foundation of China (U2004180); National Key R&D Program of China (2020YFB2008400)

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    以金属粉末为原料,采用放电等离子烧结技术制备新型含α-Al2O3的WMoNbTaV难熔高熵合金,研究了烧结温度对合金致密化行为、相结构、显微组织和耐磨性能的影响。结果表明:在1800~1900 ℃烧结时,WMoNbTaV-Al2O3高熵合金基体具有单一bcc相结构,Al2O3的平均晶粒尺寸为1.15 μm。随着烧结温度升高,合金的晶粒尺寸增大,致密度和显微硬度也在不断增高,在1900 ℃烧结时硬度达到7967.4 MPa。1900 ℃烧结得到的合金具有优异的耐磨性,磨损量仅为1800 ℃烧结合金的一半。且WMoNbTaV-Al2O3高熵合金的耐磨性远高于纯W材料。当磨料粒度为37.5 μm时,1900 ℃烧结的合金磨损量为0.9 mg,磨损性能是纯W材料的83倍。

    Abstract:

    A new refractory high entropy alloy WMoNbTaV containing Al2O3 was prepared by spark plasma sintering. The effects of sintering temperature on densification behavior, phase structure, microstructure and wear resistance of the alloy were studied. The results show that when sintered at 1800?1900 °C, the matrix of WMoNbTaV-Al2O3 has a single bcc phase structure, and the average grain size of Al2O3 is 1.15 μm. With the increase in sintering temperature, the grain size of the alloy increases, the density and microhardness also increase, and the hardness reaches 7967.4 MPa when the sintering temperature is 1900 °C. The alloy sintered at 1900 °C has excellent wear resistance, and the wear amount is only half of that of the alloy sintered at 1800 °C. The wear resistance of WMoNbTaV-Al2O3 high entropy alloy is much higher than that of pure W material. When the abrasive particle size is 37.5 μm, the wear mass loss of alloy sintered at 1900 °C is 0.9 mg, and the wear resistance of alloy is 83 times higher than that of pure W material.

    参考文献
    相似文献
    引证文献
引用本文

刘美君,徐流杰,李洲,郭明宜,胡继康,申华海.放电等离子烧结WMoNbTaV-Al2O3 高熵合金组织及磨损性能[J].稀有金属材料与工程,2024,53(5):1236~1244.[Liu Meijun, Xu Liujie, Li Zhou, Guo Mingyi, Hu Jikang, Shen Huahai. Microstructure and Wear Properties of WMoNbTaV-Al2O3 High Entropy Alloy Prepared by Spark Plasma Sintering[J]. Rare Metal Materials and Engineering,2024,53(5):1236~1244.]
DOI:10.12442/j. issn.1002-185X. E20230049

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2023-11-14
  • 最后修改日期:2024-03-18
  • 录用日期:2024-01-05
  • 在线发布日期: 2024-05-27
  • 出版日期: 2024-05-22