+高级检索
预处理对共沉淀Si3N4-Al2O3-Y2O3复合粉体的影响
DOI:
作者:
作者单位:

东北大学,东北大学,东北大学,东北大学,东北大学

作者简介:

通讯作者:

中图分类号:

基金项目:

国家自然科学基金资助(项目号51272039),中央高校基本科研任务费资助(项目号N130810003,N150203001)


Influence of Silicon Nitride composites from Coprecipitation coated powders
Author:
Affiliation:

Key Laboratory for Anisotropy and Texture of Materials of Ministry of Education ATM,Northeastern University,Key Laboratory for Anisotropy and Texture of Materials of Ministry of Education ATM,Northeastern University,Key Laboratory for Anisotropy and Texture of Materials of Ministry of Education ATM,Northeastern University,Key Laboratory for Anisotropy and Texture of Materials of Ministry of Education ATM,Northeastern University,Key Laboratory for Anisotropy and Texture of Materials of Ministry of Education ATM,Northeastern University

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    利用FTIR、SEM,TEM等手段,研究了预处理对Si3N4粉体表面基团、Zeta电位以及共沉淀法制备Si3N4-Al2O3-Y2O3复合粉体形貌的影响。结果表明:Si3N4粉体通过酸洗+950 ℃预氧化处理后,可以在粉体表面形成硅氧烷(Si-O-Si)基团,硅氧烷基团在强碱环境下水解为硅烷醇(Si-OH)基团,所得基团有利于吸附Al+和Y+离子;预处理使粉体的等电点向左偏移,当酸洗+950 ℃预氧化处理后,粉体的pHIEP<2,粉体Zeta电位在pH=9时达到-65 mV;酸洗+950 ℃预氧化处理后共沉淀粉体经过950 ℃煅烧可以制备出S3N4-Al2O3-Y2O3复合粉体,其中复合粉体中Al2O3和Y2O3的颗粒尺寸在20 ~100 nm之间。

    Abstract:

    Two types of commeriacl silicon nitride powders with poor dispersibilities have been studied, and influences of acid leaching and 950 ℃ thermal oxidation on the coprecipitation for the powders have been investigated sysmatically. The evolution of nano-oxides during the reaction causes the product to precipitation, and the calcinations of this precipitation gives nanocomposites powders(Al2O3-Y2O3) with extremely fine, uniform grains, and phase domains. microstructure properties of composites were investigated with scanning electron microscopy (SEM) (TEM) and Fourier Transform infrared spectroscopy (FTIR). The peak of the Si-O-Si groups emerge at higher frequencies after thermal oxidation, and the isoelectric point of 950 ℃ thermal oxidation powders was found to be less than 2, respectively. For the coprecipitation powders, the size of Al2O3-Y2O3 composites powders is 20~ 100nm.

    参考文献
    相似文献
    引证文献
引用本文

叶超超,姜岩,茹红强,岳新艳,王伟.预处理对共沉淀Si3N4-Al2O3-Y2O3复合粉体的影响[J].稀有金属材料与工程,2018,47(S1):298~301.[Ye Chaochao, Jiang Yan, Ru Hongqiang, Yue Xinyan, Wang Wei. Influence of Silicon Nitride composites from Coprecipitation coated powders[J]. Rare Metal Materials and Engineering,2018,47(S1):298~301.]
DOI:[doi]

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2017-07-03
  • 最后修改日期:2017-07-04
  • 录用日期:2018-01-29
  • 在线发布日期: 2018-10-22
  • 出版日期: