    Ceramic oxide coatings were fabricated on a Ti6Al4V alloy surface by micro-arc oxidation (MAO) in Na2SiO3-KOH-(NaPO3)6-NaAlO2 solution using an AC power supply. Microstructure, phase and composition of ceramic coatings were characterized by SEM and XRD respectively. Mechanical properties were studied using a Nano Indenter XP system. The results show that ceramic coatings possess three layers transitional, dense and loose layer, composed mainly of rutile TiO2 and a small amount of anatase TiO2. Elastic recovery is 40.5% and 14.9%, hardness is 8.54 GPa and 5.5 GPa, and elastic modulus is 87.4 GPa and 150 GPa in the dense layer and the substrate, respectively, The MAO coating indicates pronounced ceramic characteristics.

    Reference
    Related
    Cited by
Get Citation

[Wang Yaming, Jiang Bailing, Lei Tingquan, Guo Lixin, Cao Yueping. Microstructure and Mechanical Properties of Ceramic Coatings Produced on Ti6A14V by Micro-arc Oxidation in Na2SiO3 Solution[J]. Rare Metal Materials and Engineering,2004,33(5):502~506.]
DOI:[doi]

Copy
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:
  • Revised:September 16,2002
  • Adopted:
  • Online:
  • Published: