+Advanced Search
Preparation of P/M Ti-6Al-4V Alloy Using Hydrogenation-Dehydrogenation (HDH) Powder and Hydride Powder
DOI:
Author:
Affiliation:

Clc Number:

TG146.23

Fund Project:

  • Article
  • |
  • Figures
  • |
  • Metrics
  • |
  • Reference
  • |
  • Related
  • |
  • Cited by
  • |
  • Materials
  • |
  • Comments
    Abstract:

    Taking the process of producing MIM Ti-6Al-4V alloy by HDH powder as a reference, the processes of making P/M Ti-6Al-4V and MIM Ti-6Al-4V by using TiH2 have been discussed. When using HDH Ti powder making MIM Ti-6Al-4V the tensile strength is 819 MPa and elongation percentage is 7%. When using TiH2 powder making P/M Ti-6Al-4V the tensile strength is over 850 MPa. And when using TiH2 powder making MIM Ti-6Al-4V, processes of dehydrogenation and debinding are successfully reached.

    Reference
    Related
    Cited by
Get Citation

[Yu Lan, Li Yimin, Deng Zhongyong, Li Duxin. Preparation of P/M Ti-6Al-4V Alloy Using Hydrogenation-Dehydrogenation (HDH) Powder and Hydride Powder[J]. Rare Metal Materials and Engineering,2005,34(10):1622~1626.]
DOI:[doi]

Copy
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:June 15,2004
  • Revised:August 19,2005
  • Adopted:
  • Online:
  • Published: