    Hot compression tests of die-cast AZ91D magnesium alloy were performed on Gleeblle-1500D at strain rates ranging in 0.01~10 s-1 and deformation temperatures ranging in 250~450 oC. The constitutive equation, =1.41×1012 [sinh(0.014σ)]5.295exp (–159 449.509/RT), which is described by Zener-Hollomom parameters for hot compression deformation of die-cast AZ91D magnesium alloy was established. Compared to gravity cast AZ91D magnesium alloy, the deformation activation energy of die-cast AZ91D magnesium alloy, Q=159.45 kJ·mol-1, determined by hyperbolic sine function is lower

    Reference
    Related
    Cited by
Get Citation

[You Guoqiang, Zuo Xudong, Tan Xia, Wang Xiangjie, Long Siyuan. Flow Stress of Die-Cast AZ91D Magnesium Alloy under Hot Compression Deformation[J]. Rare Metal Materials and Engineering,2013,42(9):1844~1848.]
DOI:[doi]

Copy
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:November 28,2012
  • Revised:
  • Adopted:
  • Online:
  • Published: