Preparation of TiAl Alloy by Gel-Casting Process
DOI:
Author:
Affiliation:

Clc Number:

Fund Project:

  • Article
  • |
  • Figures
  • |
  • Metrics
  • |
  • Reference
  • |
  • Related
  • |
  • Cited by
  • |
  • Materials
  • |
  • Comments
    Abstract:

    TiAl alloy workpieces were prepared using titanium powder or titanium hydride power and aluminum powder as raw material by low-temperature sintering, gel-casting, batching out and pressureless sintering. The results show that the TiAl alloy powder can be obtained by heating titanium powder and aluminum power for 2 h at 500 oC and 3 h at 600 oC, or heating titanium hydride power and aluminum powder for 3 h at 750 oC. The last sintering process is 2 h at 1450 oC and 2 h at 1400 oC for the two kinds of processing. The relative density are 91% and 96.75%, respectively

    Reference
    Related
    Cited by
Get Citation

[Wang Zhi, Shao Huiping, Ye Qing, Lin Tao, Guo Zhimeng, He Xinbo, Zhao Yong, Lin Junpin. Preparation of TiAl Alloy by Gel-Casting Process[J]. Rare Metal Materials and Engineering,2014,43(9):2262~2266.]
DOI:[doi]

Copy
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:September 24,2013
  • Revised:
  • Adopted:
  • Online: February 25,2015
  • Published: