    Abstract:

    The ultrafine WC-0.5Co cemented carbide with a grain size smaller than 0.5 μm was prepared by high energy ball milling and HIP-sintering process. The raw materials were ultrafine WC and WC-0.5Co powder and the additives of grain growth inhibitor were VC/Cr3C2 and carbon. Microstructure and properties of the ultrafine WC-0.5Co cemented carbide with different VC/Cr3C2 and carbon contents were studied. The results show that there is a significant effect of VC/Cr3C2 on controlling WC particle size and hardness of ultrafine WC-0.5Co cemented carbide. Ultrafine WC-0.5Co cemented carbide has best Vickers hardness HV0.05 of 32 658 MPa with the VC/Cr3C2 content of 0.73% (mass fraction, similarly hereinafter). A certain amount of mixed carbon content is good for decarburization and properties of the ultrafine binderless cemented carbide. Ultrafine WC-0.5Co-073VC/Cr3C2 cemented carbide has best comprehensive mechanical properties with transverse rupture strength of 6.935 MPa·m1/2 and Vickers hardness HV0.05 of 32 216 MPa when the mixed content of carbon is 0.2%

    Reference
    Related
    Cited by
Get Citation

[Zheng Huchun, Fan Jinglian, Yang Wenhua, Zhang Zhongjian, Liu Tao. Influence of VC/Cr3C2 and Mixed Carbon Content on Microstructure and Properties of Ultrafine WC-0.5Co Cemented Carbide[J]. Rare Metal Materials and Engineering,2015,44(4):912~917.]
DOI:[doi]

Copy
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:April 13,2014
  • Revised:
  • Adopted:
  • Online: June 08,2015
  • Published: