    The microstructure, annealing strengthen and compressive deformation mechanism of Mg-5.3Nd alloy were investigated by using of OM, XRD, SEM/EDS and room temperature compression test, the results showed that the main second phase on as-casting Mg-5.3Nd alloy was Mg12Nd and the optimal solution treatment was 550 ℃×8 h for eliminating the second phases. Not subsequent unload and recompression but annealling treatment between pre-compression and recompression could markedly increase the compression strength of pre-deformed Mg-5.3Nd solid solution and the optimal annealing process was 180℃×4 h to reach the strength increament of 47MPa. The in-situ optical micrographs indicated that the preformed twins in the pre-compressed Mg-5.3Nd alloy untreated by annealing obviously grew up during the subsequent compression, whereas after annealing treatment the second compression deformation proceeded by the initiation of the new twins rather than the growth of the prefromed ones for the diffusion segregation of Nd element in the twin grainboudary during annealing process.

    Reference
    [1] Du wenbo(杜文博), Wu Yufeng(吴玉锋), Nie Zuoren (聂祚仁)et al. Rare Metal Materials and Engineering(稀有金属材料与工程)[J], 2006, 35(9): 1345
    [2] Liu W C, Dong J, Zhang P, Yao Z Y et al. Journal of Ma-terials Science[J], 2009, 44(11): 2916
    [3] Tan J C, Tan M J. Materials Science Engineering A[J], 2003, 339(1-2): 81
    [4] Guo Xuefeng(郭学锋), Yang Wenpeng(杨文朋), Ren fang(任昉)et al. Hot Working Technology(热加工工艺)[J], 2012,41(24):15
    [5] Jiang L, Jonas J J, Luo A A et al. Materials Science Engineering A[J], 2007, s 445–446(6): 302
    [6] Zhu Qiong(朱琼), Fang Canfeng(房灿峰), Li Naipu(李乃朴)et al. Rare Metal Materials and Engineering(稀有金属材料与工程)[J], 2013, 42(4): 775
    [7] Liu Zhijie(刘志杰), Wu Guohua(吴国华), Pang Song(庞松)etal. Foundry Technology(铸造技术)[J], 2012, 33(2): 151
    [8] Lü Y Z, Wang Q D, Zeng X Q et al. Mater Sci Eng A[J],2000, 278(1): 66
    [9] Li Jiehua(李杰华), Jie Wanqi(介万奇), Yang Guangyu(杨光昱). Rare Metal Materials and Engineering (稀有金属材料与工程)[J], 2010, 39(1):101
    [10] Wang Xiaoqiang(王小强), Li Quanan(李全安), Zhang Xing-yuan(张兴渊). Special Casting Nonferrous Alloys(特种铸造及有色合金)[J], 2010, 58(3): 151
    [11] Li Ting(李婷), Du Zhiwei(杜志伟), Zhang Kui(张奎)et al. Materials Review(材料导报)[J], 2012, 26(21): 96
    [12] Han Baojun(韩宝军), He Qiang(何琼), Yang Miao(杨妙).Foundry Technology(铸造技术)[J], 2014(12)
    [13] Wang Na(王娜), Lei Yiping(雷丽萍), Fang Gang(方刚)et al.Chinese Journal of Rare Metals(稀有金属)[J], 2008, 32(6):766
    [14] Jain A, Duygulu O, Brown D W et al.. Materials Science Engineering A[J], 2008, 486(1-2): 545
    [15] Reed-Hill R E, Robertson W D. Acta Metallurgica[J], 1957,5(12): 717
    [18] 王玮. Multistage purification behavior for Mg-10Gd-3Y-0.5Zr alloy(Mg-10Gd-3Y-0.5Zr合金复合净化行为研究)[D]. Shanghai: Shanghai Jiao Tong University. 2010
    [19] Nodooshan H R J, Liu W, Wu G et al. Journal of Alloys Compounds[J], 2015, 619(619): 826
    [20] Mirza F A, Chen D L, Li D J et al. Materials Design[J], 2012, 46(4): 411
    [21] Xia Changqing(夏长清), Wu Wenhua(武文花), Wu Anru(吴安如)et al. The Chinese Journal of Nonferrous Metals(中国有色金属学报)[J]. 2001, 14(11): 1810
    [22] Li Jiehua(李杰华), Jie Wanqi(介万奇), Yang Guangyu(杨光昱). Rare Metal Materials and Engineering(稀有金属材料与工程)[J], 2008, 37(10):1751
    [23] Zeng Z R, Zhu Y M, Bian M Z et al. Scripta Materialia [J], 2015,107: 127
    [24] Chen Jian, Wang Zhaoqiang, Ma Xiaoguang et al. Journal of Alloys and compounds[J], 2015, 642: 92
    [25] Zhan Meiyan(詹美燕), Li Chuanming(李春明), Shang Junling(尚俊玲). [J]. Materials Review(材料导报), 2011(3): 1
    [26] Wang Zhongtang(王忠堂), Yan Cao(严操), Song Guangsheng(宋广胜)et al. Metal Materials and Engineering(稀有金属材料与工程)[J], 2012, 41(2): 221
    [27] Bohlen J, Chmel F, Dobro P et al. Journal of Alloys and Compounds[J], 2004, 378: 207
    [28] Nie J F, Zhu J Z et al. Science[J]. 2013, 340(6135): 950
    [29] Kadiri H E, Kapil J, Oppedal A L et al. Acta Materialia[J],2013, 61(10): 214
    [30] Zhang Jing, Dou Yuchen, Zheng Yi. Scripta Materialia[J], 2014, 80: 17
    [16] Guo ruihua(郭瑞华), Liu yucheng(刘玉乾), Zhang jieyu(张捷宇). Heat treatment of metals (金属热处理)[J], 2016, 41(6):51.
    [17] Su zaijun(苏再军), Yang shuzhong(杨树忠,) Pu jian(普建). Hot Working Technology (热加工工艺)[J], 2016,45(9):15
    Cited by
    Comments
    Comments
    分享到微博
    Submit
Get Citation

[Yao Yu-hong, He Yi-ke, Chen Jian, Wang Wei, Liu Jiang-nan. Annealing treatment on compress strength of pre-deformed Mg-5.3Nd alloy[J]. Rare Metal Materials and Engineering,2016,45(11):2999~3003.]
DOI:[doi]

Copy
Article Metrics
  • Abstract:1350
  • PDF: 1366
  • HTML: 138
  • Cited by: 0
History
  • Received:June 22,2016
  • Revised:September 01,2016
  • Adopted:September 14,2016
  • Online: December 08,2016