Effect of Micro/nano-SiCP on Microstructure and Properties of Electroless Ni-P-SiCP Composite Coatings
Author:
Affiliation:

1.School of Mechanical and Equipment Engineering, Hebei University of Engineering, Handan 056038, China;2.Key Laboratory of Intelligent Industrial Equipment Technology of Hebei Province, Handan 056038, China;3.School of Mechanical and Electrical Engineering, China University of Mining and Technology (Beijing), Beijing 100083, China;4.Department of Aeronautical and Automotive Engineering, Loughborough University, Loughborough LE11 3TU, UK

Clc Number:

Fund Project:

Science Research Project of Handan Bureau of Science and Technology (21422075242)

  • Article
  • |
  • Figures
  • |
  • Metrics
  • |
  • Reference
  • |
  • Related
  • |
  • Cited by
  • |
  • Materials
  • |
  • Comments
    Abstract:

    Ni-P-SiCP coatings were deposited on 42CrMo steel by electroless plating. The surface morphologies and phase structures of the Ni-P-SiCP coatings processed under different SiCP concentrations at different heat treatment temperatures were analyzed. The microhardness, corrosion resistance, and wear resistance of the Ni-P-SiCP coatings were studied. Results show that Ni-P-SiCP coatings exhibit cauliflower-like morphology. Increasing the SiCP concentration can reduce the size of cellular structure. The microhardness and corrosion resistance are initially increased and then decreased with the increase in SiCP concentration. The maximum microhardness and corrosion potential are 7379 MPa and -0.363 V, respectively, when the SiCP concentration is 5 g/L. The Ni-P-SiCP coatings exhibit an amorphous structure, and the width of the diffuse diffraction peak becomes narrower with the increase in SiCP concentration. It is suggested that SiCP inhibits the deposition of P and promotes the microcrystalline transformation. After heat treatment at 350 °C, the Ni-P-SiCP coatings are crystallized, resulting in the precipitation of Ni3P phase. Heat treatment at 400 °C for 1 h maximizes the structure. The synergistic effect of the Ni3P precipitate phase and SiCP dispersion phase promotes the densification of the cellular structure, leading to the optimal microhardness (13 828 MPa), optimal corrosion resistance (-0.277 V), and excellent wear resistance. The wear mechanism is dominated by micro-cutting abrasive wear with slight adhesive and oxidative wear.

    Reference
    Related
    Cited by
Get Citation

[Chao Shuang, Cao Jingjing, Li Hezong, Fan Lei, Yang Junheng, Martin Harvey Christopher. Effect of Micro/nano-SiCP on Microstructure and Properties of Electroless Ni-P-SiCP Composite Coatings[J]. Rare Metal Materials and Engineering,2024,53(10):2723~2734.]
DOI:10.12442/j. issn.1002-185X.20240245

Copy
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:April 25,2024
  • Revised:April 27,2024
  • Adopted:May 08,2024
  • Online: September 27,2024
  • Published: September 27,2024