Microstructure and Properties of Al-Zn-Mg-Cu-Zr Alloy with Low Scandium Content
Author:
Affiliation:

1.School of Marine Equipment and Mechanical Engineering, Jimei University, Xiamen 361021, China;2.Hunan Engineering Research Center of Forming Technology and Damage Resistance Evaluation for High Efficiency Light Alloy Components, Hunan University of Science and Technology, Xiangtan 411201, China;3.Jiangxi Copper Technology Research Institute Co., Ltd, Nanchang 330096, China;4.School of Materials Science and Engineering, Guangdong Ocean University, Yangjiang 529500, China;5.Light Alloy Research Institute, Central South University, Changsha 410083, China

Clc Number:

TG135+.1;TG146.21

Fund Project:

National Natural Science Foundation of China(52475356、52471132、52471055、52475357、U21A20130)、Natrual Science Foundation of Jiangxi Province for Distinguished Young Scholars(20224ACB218002)、Natrual Science Foundation of Fujian Province for Distinguished Young Scholars (2024J010031)

  • Article
  • |
  • Figures
  • |
  • Metrics
  • |
  • Reference
  • |
  • Related
  • |
  • Cited by
  • |
  • Materials
  • |
  • Comments
    Abstract:

    The relationship between the mechanical properties and precipitation behavior of Al-Zn-Mg-Cu-Zr aluminum alloys with low Sc content (0.02wt%, 0.07wt%, 0.12wt%) was investigated by OM, SEM, TEM, and universal material testing machine. With the increase in Sc content, microstructure of as-cast alloy is gradually refined, and the coarse secondary phase at the grain boundary increases, thus weakening the effect of fine grain strengthening. In the alloy at rolling+T6 state, the Al3(Sc,Zr) phase inhibits the precipitation of the main strengthening phase η', and the inhibition effect becomes more obvious with the increase in Sc content, thus weakening the precipitation strengthening effect. The grain refinement is conducive to the formation of more and finer dimples during the tensile deformation, thus improving the ductility of the alloy. The low Sc content alloy (0.02wt%) shows the excellent mechanical properties after rolling and T6 heat treatment, whose tensile strength and elongation are 683 MPa and 21%, respectively.

    Reference
    Related
    Cited by
Get Citation

[Zhu Biwu, Xiao Gang, Liu Xiao, Ye Fan, Zhang Wei, Cui Xiaoli, Zhan Haihong, Liu Wenhui. Microstructure and Properties of Al-Zn-Mg-Cu-Zr Alloy with Low Scandium Content[J]. Rare Metal Materials and Engineering,2025,54(3):722~729.]
DOI:10.12442/j. issn.1002-185X.20240552

Copy
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:August 26,2024
  • Revised:November 18,2024
  • Adopted:December 02,2024
  • Online: March 25,2025
  • Published: March 25,2025