    Abstract:

    Porous tantalum materials were prepared by a vacuum sintering technique using fine tantalum powder (< 0.45 μm) as the starting raw material. Effects of sintering time (10, 20, 30, 40 and 50 min) at 1250 oC on the microstructures and the porous characteristics of the porous tantalum were investigated. The results show that the porous tantalum materials have the porosity of about 50% with pore size distribution of 0.08 cm3/g

    Reference
    Related
    Cited by
Get Citation

[Shi Wei, Yang Bangchao, Zhang Xuanhong, Ma Jianhua, Pan Qifeng, Wang Xingwei. Effect of Sintering Time on the Microstructure of Porous Tantalum[J]. Rare Metal Materials and Engineering,2015,44(2):319~322.]
DOI:[doi]

Copy
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:March 05,2014
  • Revised:
  • Adopted:
  • Online: May 29,2015
  • Published: