    Abstract:

    Ti-6Al-4V(wt.%)/Ti-43Al-3V-2Cr(at.%) composite plates with no interfacial defects were successfully prepared by a high-reduction hot-rolling method. Microstructure and mechanical properties were studied. The experimental results show that no obvious defects in the interfacial region are observed, and the Kirkendall phenomenon is successfully avoided. The interface thickness of the composite plate is about 230 μm, according to different phase compositions, the interface is divided into two regions, one of which is near the interface of Ti6Al4V alloy and is mainly composed of α/α2 + β/B2 phase; Interface 2 is near the interface of TiAl alloy, and mainly consists of α/α2 + β/B2 + γ phase. The interface region structure is due to the diffusion of Ti element in Ti6Al4V alloy to TiAl alloy layer and the diffusion of Al and Cr elements from TiAl layer to Ti6Al4V alloy layer. The Vickers hardness and three-point flexural strength of the composite panels were tested with different loading methods. The experimental results show that the interface 1 has the highest microhardness, and the composite plate exhibits the best bending resistance when the surface of the transverse specimen is loaded, and the bending strength reaches 1150.82 MPa. The mechanical properties were analyzed and discussed in detail in combination with the microstructure characteristics.

    Reference
    [1] J. Hirsch, T. Al-Samman, Acta. Materialia[J]. 2013, 61: 818-843
    [2] D. J. Harvis, D. Voss, Materials Science and Engineering:A[J]. 2005,413-414: 583-591
    [3] F. Appel, R. Wagner, Materials Science and Engineering:A[J]. 1998,22(5): 187-268
    [4] M. Yamaguchi, Y. Umakoshi, Progress in Materials Science[J]. 1990,34(1): 1-148
    [5] F. Appel, R. Wagner, Materials Science and Engineering:A[J]. 1998, 22(5): 187-268
    [6] H.L. Yu, C. Lu, A.K. Tieu et al. Materials Science and Engineering: A[J]. 2016, 660: 195-204
    [7] P.J. Zhou, C.H. Guo, E.H. Wang et al. Materials Science and Engineering: A[J]. 2016, 665: 66-75
    [8] Qiu Xiaotun , Liu Ranran ,Guo Shengmin et al. Metallurgical and Materials Transactions A[J]. 2009, 40: 1541-1546
    [9] Ramaseshan R, Kakitsuju A, Seshadri S K et al. Intermetallics [J]. 1999, 7(5): 571-577
    [10] Sun Yanbo(孙彦波),Zhao Yeping(赵业青),Zhang Di(张迪) et al. Transactions of Nonferrous Metals Society of China[J]. 2010, 20(S1): 1064-1067
    [11] Sun Wei, Yang Fei, Kong Fantao et al. Materials Characterization[J]. 2018, 144: 173-181
    [12] Kong Fantao, Chen Yuyong, Zhang Deliang.Materials & Design[J]. 2011, 32(6): 3167-3172
    [13] Sun Wei, You Fenghai, Kong Fantao et al. Journal of Alloys and Compounds[J]. 2020, 820: 153088
    [14] D.V. Lazurenko, I.A. Bataev, V.I. Mali et al. Materials & Design[J]. 2016, 102: 122-130
    [15] G.P. Chaudhari, V.L. Acoff. Intermetallics[J]. 2010, 18(4), 472-478
    [16] Foadian F, Soltanieh M, Adeli M et al. Metallurgical and Materials Transactions A[J]. 2014, 45(4): 1823-1832
    [17] Kong Fantao(孔凡涛), Chen Yuyong(陈玉勇), Wang Wei(王威) et al. Transactions of Nonferrous Metals Society of China[J]. 2009, 19(05): 1126-1130
    [18] R.V.Ramanujan. International Materials Reviews[J]. 2000, 45(6): 217-240
    [19] Charpentier M,Daloz D,Gautier E et al. Metallurgical and Materials Transactions A[J]. 2003, 34: 2139-2148
    [20] Xinhua Wu. Intermetallics[J]. 2006, 14(10-11): 1114-1122
    [21] Takeyama M, Kobayashi S. Intermetallics[J]. 2005, 13(9): 993-999
    [22] Kong Fantao(孔凡涛), Chen Yuyong(陈玉勇). Rare Metal Materials and Engineering[J]. 2009, 38(8): 1484-1486
    [23] Yu Z, Wang X, Kong F et al. Materials[J]. 2017, 10(9): 1089
    [24] Liu H, Li Z, Gao F et al. Journal of Alloys & Compounds[J]. 2017, 698: 898-905
    [25] 孙巍. 哈尔滨工业大学[D]. 2016
    [26] Yamabe Y, Takeyama M, Kikuchi M. Minerals, Metals and Materials Society, Warrendale, PA (United States)[R]. 1995,No. CONF-950201
    [27] Zghal S, Naka S, Couret A. Acta Materialia[J]. 1997, 45(7): 3005-3015
    [28] Jaffee R I. The Science, Technology and Application of Titanium[M]. 1970
    [29] R.R. Boyer, R.D. Briggs. Journal of Materials Engineering and Performance[J]. 2005, 14: 681-685
    [30] Y.Wang, K.S.Vecchio, Materials Science and Engineering:A[J]. 2016, 649(1): 325-337
    [31] Niu H Z, Kong F T, Chen Y Y et al. Journal of Alloys and Compounds[J]. 2011, 509(42): 10179-10184
    [32] Wei S, Fy C, Fka B et al. Intermetallics[J]. 2020, 118: 106684
    Cited by
Get Citation

[Wang Hao, Gao Tianbao, Wei Junxin, Zhang Mengfei, Deng Ruijun, Jia Yi, Han Jianchao. Study on Hot Rolling Bonding Behavior and Microstructure and Properties of Ti/TiAl Clad Plate under Large Reduction[J]. Rare Metal Materials and Engineering,2023,52(7):2485~2493.]
DOI:10.12442/j. issn.1002-185X.20220543

Copy
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:June 24,2022
  • Revised:May 26,2023
  • Adopted:August 12,2022
  • Online: August 09,2023
  • Published: July 27,2023